Electrode
cooling:
Nozzle cooling:
Weldable
material thickness:
Max. current-carrying capacity
with
Electrode on - polarity:
Duty cycle:
Powder particle size:
Powder deposition rate:
Plasma gas:
Shield gas: |
|
indirect
water-cooled
indirect water-cooled
0,05 up to 4mm
100A 100 % -200 +60µm 20g/min. Argon
Argon, Argon/Hydrogen |